[1] AL SHAWAF A H, MAITY M K. High Temperature Alloys Failures in the Petrochemical Furnaces[C/OL]. (2018-04-15)[2025-01-23]. https:∥content.ampp.org/nace/proceedingsabstract/CONF_APR2018/2018/1/58171.
[2] HAN Z, XIE G, CAO L, et al. Material Degradation and Embrittlement Evaluation of Ethylene Cracking Furnace Tubes after Long Term Service[J]. Engineering Failure Analysis, 2019,97:568-578.
[3] JAKOBI D, GOMMANS R. Typical Failures in Pyrolysis Coils for Ethylene Cracking[J]. Material Corrossion, 2003,54(11):881-887.
[4] GUAN K, XU H, WANG Z. Analysis of Failed Ethylene Cracking Tubes[J]. Engineering Failure Analysis, 2005,12:420-431.
[5] KUS S,LOHAKARE D, DIVAKARAN V, et al. Failures of High Temperature Alloys in Ethylene Furnaces—Case Studies[C/OL]. (2014-03-09)[2025-01-23]. https:∥onepetro.org/NACECORR/proceedingsabstract/CORR14/AllCORR14/NACE20144202/123075.
[6] 陈涛, 陈学东, 刘春娇, 等. 裂解炉管初生碳化物分类及对高温持久性影响[J]. 机械工程学报, 2018,54(8):109-116.
[7] 蒋明敬. 乙烯装置气体原料裂解炉炉管异常分析[J]. 石油化工设备技术, 2021,42(2):47-51,55.
[8] 刘建杰,储拥军,陈俊海,等. 乙烯裂解炉静态铸造管件射线检测影像研究[J]. 石油化工设备技术, 2019,40(1):34-37.
[9] 郑显伟. 我国乙烯裂解炉辐射炉管的使用状况[J]. 压力容器, 2013,30(5):45-52.
[10]FACCO A, COUVRAT M, MAGN D, et al. Microstructure Influence on Creep Properties of HeatResistant Austenitic Alloys with High Aluminum Content[J]. Materials Science and Engineering: A, 2020,783:139276.
[11]SHI S, LIPPOLD J C. Microstructure Evolution during Service Exposure of Two Cast, HeatResisting Stainless Steels—HPNb Modified and 2032Nb[J]. Materials Characterization, 2008,59:1029-1040.
[12]ULHAMID A, TAWANCY H M, MOHAMMED A R I, et al. Failure Analysis of Furnace Radiant Tubes Exposed to Excessive Temperature[J]. Engineering Failure Analysis, 2006,13:1005-1021.
[13]BABAKR A M, ALAHMARI A,ALJUMAYIAH K, et al. Sigma Phase Formation and Embrittlement of Cast IronChromiumNickel (FeCrNi) Alloys[J]. Journal of Minerals and Materials Characterization and Engineering, 2008,7(2):127-145.
[14]MOBARAKI M,AFSHANG B, RAHIMPOUR M R, et al. Effect of Cracking Feedstock on Carburization Mechanism of Cracking Furnace Tubes[J]. Engineering Failure Analysis, 2020,107:104216.
[15]ASRAR N, ASHIRU O A, A1BEED A. Erosion Damages of High Temperature and Wear Resistant Materials during Ethylene Cracking in a Petrochemical Plant[C/OL]. (2000-03-26)[2025-01-23]. https:∥onepetro.org/NACECORR/proceedingsabstract/CORR00/AllCORR00/NACE00087/111850.
[16]杨帆,刘辉,苗壮,等. 22万 t/a乙烯装置的裂解炉长周期运行与设备管理[J]. 石油化工设备技术, 2020, 41(4):63-66.
[17]IRFAN M A, CHAPMAN W. Thermal Stresses in Radiant Tubes Due to Axial, Circumferential and Radial Temperature Distributions[J]. Applied Thermal Engineerign, 2009,29:1913-1920. |